Sheets, Plates & Coils |
|
|
|
|
- Ravi Ratan Metal Industries supplies heavy plates, alloy steel coils, carbon steel coils, alloy steel sheets, hot rolled coils.
- Both steel plate and hot rolled coils satisfy the more important needs from a technological and dimensional point of view.
|
|
Plate |
Thickness : to a maximum of 200 mm;
Width : from 1250 mm to 2500 mm. |
Coil |
Thickness : to a maximum of 20 mm;
Width : up to a maximum 2000 mm |
|
Chemical Composition of Sheets/ Plates |
ASTM |
Grade |
C max |
Mn max |
P max |
S max |
Si max |
Ni |
Cr |
Mo |
A 515 |
60 |
0.27 |
0.9 |
0.04 |
0.04 |
0.15.04 |
|
|
|
70 |
0.33 |
1.2 |
0.04 |
0.04 |
0.15-0.40 |
|
|
|
A 516 |
60 |
0.23 |
0.85-1.20 |
0.04 |
0.04 |
0.15-0.40 |
|
|
|
|
70 |
0.28 |
0.85-1.20 |
0.04 |
0.4 |
0.15-0.40 |
|
|
|
A 537 |
Class 1 |
0.02 |
0.70-1.35 |
0.04 |
0.04 |
0.15-0.40 |
0.25max |
0.80 max |
0.35max |
Class 2 |
0.24 |
0.70-1.35 |
0.04 |
0.04 |
0.15-0.40 |
0.25 max |
0.80 max |
0.35max |
|
|
Mechanical Requirements |
Hardness |
ASTM |
Grade |
Tensile Strength Apa (ksi) min |
Yield Strength Mpa (ksi)min |
Elongation min% |
Brinel max HB |
Rockwell max HRB |
A 515 |
60 |
415-550/(60-80) |
220(32) |
25 |
_ |
_ |
70 |
485-620/(70-90) |
260(38) |
21 |
_ |
_ |
A 516 |
60 |
415-550/(60-80) |
220(32) |
25 |
_ |
_ |
70 |
485-620/(70-90) |
260(38) |
21 |
_ |
_ |
A 537 |
Class 1 |
485-620/(70-90) |
345(50) |
22 |
_ |
_ |
Class 2 |
550690/(80-100) |
415-60 |
22 |
_ |
_ |
|
Chromoly is an abbreviation for "chromium-molybdenum steel". Chromoly is an alloy used to produce tubing for bicycle frames and race-car roll cages. It is not as lightweight as some steel alloys, but has the advantages of high tensile strength and malleability. It is also easily welded and is considerably stronger and more durable than standard (1020) steel tubing. |
Chemical Composition of Sheets/ Plates |
ASTM |
Grade |
C max |
Mn max |
P max |
S max |
Si max |
Ni |
Cr |
Mo |
Others |
A387 Class 1 Class 2 |
5 |
0.15 |
0.30-0.60 |
0.04 |
0.03 |
0.5 |
|
4.00-6.00 |
0.45-0.65 |
|
|
9 |
0.15 |
0.30-3.60 |
0.03 |
0.3 |
1 |
|
8.00-10.0 |
0.90-1.10 |
|
|
11 |
0.04-0.17 |
0.40-0.65 |
0.04 |
0.04 |
0.50-0.80 |
|
1.00-1.50 |
0.45-0.65 |
|
|
12 |
0.04-0.17 |
0.40-0.65 |
0.04 |
0.04 |
0.15-0.40 |
|
0.80-1.15 |
0.45-0.60 |
|
|
22 |
0.05-0.17 |
0.30-0.60 |
0.04 |
0.035 |
0.5 |
|
2.00-2.50 |
0.90-1.10 |
|
|
|
|
Mechanical Requirements |
Hardness |
ASTM |
Grade |
Tensile Strength Apa (ksi) min |
Yield Strength Mpa (ksi)min |
|
Elongation min% |
Brinel max HB |
Rockwell max HRB |
|
|
Class 1 |
Class 2 |
Class1 |
Class2 |
|
|
|
A387 Class 1 Class 2 |
5 |
415-585 |
515-690 |
205 |
310 |
18 |
202 |
92 |
9 |
415-585 |
515-690 |
205 |
310 |
18 |
217 |
95 |
11 |
415-585 |
515-690 |
240 |
310 |
22 |
217 |
95 |
12 |
380-550 |
450-585 |
230 |
275 |
22 |
217 |
95 |
22 |
415-585 |
515-690 |
205 |
310 |
18 |
201 |
92 |
|